Blog
- Details
TestResources offers both servo hydraulic test machines and electrodynamic test machines. The two types of test machines are functionally identical, using the same high performance 24 bit resolution test controller. Servo hydraulic technology is older - first applied to testing in 1958. TestResources first electrodynamic test machine was delivered in 2003 and is still functioning and in use performing dental implant fatigue tests and research at New York University.
1. A major difference between the two types of machines is that the load and displacement performance of a servohydraulic actuator (depending on power pack size), can be configured to deliver higher forces at higher speeds. Servohydraulic actuators can deliver loads up to 3 mN (670 kip). Low force actuators can perform tests at speeds to 200 hz.
2. The purchase, operating and maintenance costs of Electrodynamic solutions are significantly lower than Servo Hydraulic test machines. Lower force M Series linear motors perform high speed tests to 100 hz. E series actuators deliver forces to 100 kN (22 kip) at test speeds in excess of 15 hz.
3. Electrodynamic test machines all use noise free high resolution digital position encoders which deliver improved control quality and long term stability over servohydraulic test machines that use LVDT’s. Recent developments have made it possible to configure encoders on servo hydraulic actuators.
4. Competing controllers resolve data to 16 bits and TestResources controllers resolve to 24 bit, which is 256 times more than 16 bit. In addition, electrodynamic actuators are much easier to tune and much more stable in lower speed applications.
5. Servo hydraulic test machines are inherently noisy and all leak oil at some level. Electro dynamic systems are quiet and reliable.
- Details
Dog bone tensile test samples are primarily used in tensile tests. The sample has a shoulder at each end and a gauge section in between. The shoulders are wider than the gauge section which causes a stress concentration to occur in the middle when the sample is loaded with a tensile force. This stress concentration ensures a higher probability that the sample will rupture away from the ends. When the rupture of a sample occurs in the midsection it is attributed to the material reaching its maximum tensile strength whereas if the sample ruptures at one of the ends or in the grip itself the failure may be attributed to improper loading or a pre-existing defect in the material. Therefore a dog bone sample is designed to ensure the highest probability that the sample will fail due to maximum tensile loading.
There are several different methods that may be used to create dog bone samples. Most of these methods fall into two categories: cutting and molding.
To cut a sample from a sheet of material requires a cutting die manufactured with the appropriate dimensions. Depending on the hardness of the material the actual method of cutting the sample with the die may range from simply pushing it into the material like a cookie cutter into dough to stamping it with the aid of a hammer or mallet to pressing it through the material using a vice grip. All of these methods will produce a test sample with the shape and dimensions of the die cutter used.
Molding a test sample requires a slightly more complicated process and is generally more expensive than cutting test samples. The molding process requires the test sample to begin in a soft flexible state that usually means it is at a higher temperature than the testing temperature. The material is then either pressed or poured depending on its state into the mold of the desired sample shape and allowed to harden until it is deemed ready for testing. Specimens formed in this manner are usually stiffer than those created using the cutting method.
A dog bone test sample can be composed of any material that may be tested in tension but are usually made from plastics polymers textile fabrics or rubber. The cutting method is used to create samples from flexible material as it is easier to push the cutter through them without cracking the sample due to their ductile nature. Metals and ceramics are generally more brittle and so are molded into test samples. A metal is heated until it liquefies and is then poured into the molded whereas ceramics are molded into dog bone shapes before they are cured. Follow this link to see our customizable dogbone tensile test sample cutting die.
- Details
Tensile testing refers to testing a material property such as ultimate tensile strength, yield strength, yield limit, yield point, elastic limit, proportional limit, Poisson’s ratio, modulus of elasticity or modulus of rigidity. Tensile tests tend to be performed on standardized (e.g. ASTM or ISO) test geometries and test methods that produce materials properties data.
Tension testing refers to the force a material experiences when a load is applied in an effort to attempt to lengthen, elongate or pull the material apart. It refers to the test machine direction of force being applied and is the opposite of compression testing. A simple analogy of tension is the force experienced by a bar as both ends are pulled away from each other or the force a rubber band feels when it is stretched.
- Details
Plotting tensile stress-strain curves depicts the entire behavior of a sample as it is loaded in tension from the onset of the load to the final failure of the sample.
The sample stress (psi MPa) is equal to the load divided by the surface area to which the load is applied; sample strain is equal to the change in the sample’s length divided by the original length. Initially the loading of the sample takes place in the linear elastic region of the curve in which the sample behaves according to Hooke’s law where the ratio of stress to strain remains constant. In this region of loading the information needed to determine both the modulus of elasticity and rigidity as well as Poisson’s ratio is contained. Once the material reaches its yield point at which the yield limit and strength may be determined it will no longer return to its original shape when unloaded and switches from the elastic deformation region to the plastic deformation region of loading. This region contains the information needed to determine the ultimate tensile strength of the material. After this the material quickly enters the region of necking where the gage length begins to narrow and then finally fractures at which the test is ended.
Depending on the whether or not the material behaves in a brittle or ductile manner the fracturing may occur very quickly without much necking or a relatively long period of time in which noticeable necking occurs.
More Articles …
- The Difference between Tensile Test and Compression Test Equipment
- Tensile Test Properties
- Is a THREE Point Test the Same as a THIRD Point Test?
- Differences Between Three Point and Four Point Bending Tests
- Similarities Between a Flexural Test and Tensile Test?
- Is a THREE Point Test the Same as a THIRD Point Test?
- Why Not to Use a Handheld Force Gauge on a Peel Test
- Measuring the Modulus of Elasticity When Testing Plastics
- The Challenge of Testing Tiny Test Samples
- Differences Between a Flexure Test and Bend Test
- Typical Flexure Test Sample Geometry
Need Help?
Talk to one of our Application Engineers to help you find the right solution for your test applications